( 二 〇 一 年 十月 Abstract In conventional metal hot extrusion process, as a result of the blank shape and the uneven distribution of temperature, causes the product size, shape, microstructure and mechanical properties, such as nonuniformity, and the isothermal extrusion for decreasing the inhomogeneity, is an ideal method. In the course of the extrusion, extrusion die die deformation zone near the metal temperature is always constant or basic constant, in order to keep the uniformity of deformation resistance and flow of metal in the, so that the parts material obtain more uniform structure and