quality of joint surface
quality of joint surface, and should be uneven burnish is flat and level.
3) weldment group of former groove surface and its inside and outside surface shall be not less than 10 mm within the scope of the oil, paint, scale, rust, burr and other impurities, such as clean, and shall not have defects such as cracks, mezzanine, unqualified nozzle should be trimmed.
4) in addition to the design rules need to pipe cold drawing or cold compression, forcibly group of weldment are strictly prohibited.
5). The outer diameter and wall thickness of the same pipe or tube wrong, should be leveled, the ou