STD 5700,21去氢脆
Hydrogen embrittlement
Relief 去氢脆
Orientation 定位
This issue differs from issue 2 in that sections 1 Definition
and 2 Application have been revised and replaced
by section 1 Scope and field of application.
1 Scope and field of application
This standard describes the heat treatment of certain 本标准描述了用于降低特定钢的
steels for the purpose of reducing the risk of hydrogen- 氢致延缓断裂危险的热处理,这种
induced delayed fractures which may occur on 可能发生在一些静态收缩的零件上。
components that are statically restrained. The fractures 断裂一般在施加应力的1-24小时内发
usually occur 1 to 24 h after application of the 生。
stress.