HR3C钢高温时效过程中的析出相 图文精.docx

750 750 750 750 467 Vol.46 No.7 2010 7 844—849ACTA METALLURGICA SINICA Jul. 2010 pp.844 —49 公属总堆 HR3C ? 1 1 1,2 1 , 116085 2 , 116085HR3C (T (T 500h HR3C M 23C 6 NbCrN, M 23C 6 ,NbCrN J M 23C 6 NbCrN HR3C M 23C 6 3 J J M 23C 6 Cr HR3C TG132.33 A 0412- 1961(201007- 0844- 06 PRECIPITATES IN HR3C STEEL AGED AT HIGH TEMPERATURE FANG Yua nyua n 1 ,ZHAO Jie 1 ,LI Xiaona 2 School of Material Scie nee and Engin eeri ng, Dalia n Uni versity of Tech no logy, Dalia n 116085 Key Laboratory of Materials Modi?eati on by Laser, I on and Eleetron Beams of Ministry of Education Dalian University of Technology,