X射线衍射法测定高岭石合成的NaY分子筛物相组成、
结晶度、晶胞参数及硅铝比研究
程群(北京普析通用仪器有限责任公司北京 100081)由高岭石合成的NaY分子筛经如下处理:将试样放入玛瑙研钵中充分研细,经120℃,1小时烘干,置于氯化钙过饱和水溶液气氛中(室温℃)X射线衍射仪XRD)进行测定,分析其组成从而可以及时监控合成NaY分子筛的生产过程Study on Determining Composition, crystallinity, cell parameter and ratio of silicate to aluminium of Zeolite NaY treated from kaolinite by X-ray Diffractometer
Abstract: In this paper, Zeolite NaY treated from kaolinite continued to be treated, such as ground in the agate mortar , dried in 120℃ for an hour, damped in the surroundings of supersaturated calcium chloride solution(room temperature from 20℃ to 30℃) for 16 to