Sticky problem Many breaks on predryer, sizer coating section 在前烘、表胶、涂布段断纸太多。 Date Author Title INTERNAL * The web is sticking on cylinder surface between 1st, 2nd, 3rd cylinders. This are causing breaks, because some of the fibres are sticking to the cylinder. Than there are hole in the base layer. After that the web will be get wet and breaks on sizer or coating section.前烘1、2、3#烘缸表面胶粘物太多,这会引起断纸。因为纸会被胶粘下来从而形成孔洞。这样就会在表胶或涂布段断纸。 Reasons for sticky: 胶粘物多的原因 The cylinder temperature differences were too high.这些烘缸的温差太大 Also the temperature were too high前烘一组二组烘缸温度太高 The doctor blades were old.刮