1
LiFePO4 and C-LiFePO4 were prepared using stoichiometric
Li2CO3 (99.95%), FeC2O4·H2O (99%), NH4H2PO4 (98%), and glucose
(99%). The starting materials were first precalcined at 400 ?C for
6 h in flowing ultra-pure Ar in order to decompose the carbonate,
oxalate, and ammonium. After cooling down, the decomposed
mixtures were pressed into pellets ( 20mm, L 10mm, 10 kN) and
transferred to quartz tubes, which were then sealed in vacuum.
The vacuum-sealed sampleswere then calcined in amuffle furnace.
The quartz tubes with the samples were remov