工业分析以及马弗炉实用第1页/共41页第2页/共41页Test standardThe received sample was cut, milled and sieved (对收到基进行切割、粉碎、筛分)External water content:drying oven 、55℃ (进行外水测量:烘箱、55℃) Wad=the lost mass/total mass×100 ,% (Wad=失水量/生物质重×100 ,%)every test was set one sample in parallel(在试验中每个生物质样设置两个平行样)— 流化床及生物质能课题组 —第3页/共41页Test standardInternal water content:1g、crucible、drying oven、105℃、3h、remove to a desiccator, cool to room temperature、weigh the residue (内水测量:1g、小方舟、烘箱、105℃、3h、干燥器内冷却至室温、称重) Wad=the lost mass/total mass×100 ,% (Wad=失水量/生物质重×100 ,% )第4页/共41页Test standardAsh centent:1g、 crucible 、muffle furnace、550℃、4h