Steel structure and equipment after contact with pouring material surface

Steel structure and equipment after contact with pouring material surface, the floating rust should be removed and sundry. Shall not be arbitrarily change the ratio of castable or optional in blended castable with water or other materials. (2) the key points of technical requirements in construction 1. Stir refractory castable water should use clean water. 2. Pouring with template should have enough stiffness and strength, the mould dimension should be accurate, and should prevent deformation in the process of construction. Template seams should be tight, do not leak slurry. The template a