- 1、原创力文档(book118)网站文档一经付费(服务费),不意味着购买了该文档的版权,仅供个人/单位学习、研究之用,不得用于商业用途,未经授权,严禁复制、发行、汇编、翻译或者网络传播等,侵权必究。。
- 2、本站所有内容均由合作方或网友上传,本站不对文档的完整性、权威性及其观点立场正确性做任何保证或承诺!文档内容仅供研究参考,付费前请自行鉴别。如您付费,意味着您自己接受本站规则且自行承担风险,本站不退款、不进行额外附加服务;查看《如何避免下载的几个坑》。如果您已付费下载过本站文档,您可以点击 这里二次下载。
- 3、如文档侵犯商业秘密、侵犯著作权、侵犯人身权等,请点击“版权申诉”(推荐),也可以打举报电话:400-050-0827(电话支持时间:9:00-18:30)。
- 4、该文档为VIP文档,如果想要下载,成为VIP会员后,下载免费。
- 5、成为VIP后,下载本文档将扣除1次下载权益。下载后,不支持退款、换文档。如有疑问请联系我们。
- 6、成为VIP后,您将拥有八大权益,权益包括:VIP文档下载权益、阅读免打扰、文档格式转换、高级专利检索、专属身份标志、高级客服、多端互通、版权登记。
- 7、VIP文档为合作方或网友上传,每下载1次, 网站将根据用户上传文档的质量评分、类型等,对文档贡献者给予高额补贴、流量扶持。如果你也想贡献VIP文档。上传文档
查看更多
电解液抛光(国外英文资料)
电解液抛光(国外英文资料)
Electrolyte index:
(1) electrolyte density: 1.68-1.72
(2) electrolyte state: microyellow transparent liquid
(3) the PH: 7
(4) electrolyte working voltage: 5-9v
(5) the current density in the electrolyte (unit per square meter), 200 series 15-25 amperes, 300 series 10-15 amperes, 400 series 20-30 amperes.
(6) electrolysis time: 5-10 minutes.
(7) electrolysis per kilogram of processing area: 2 to 4 square, because the material difference processing surface area is different.
(8) the electrolyte temperature: 50-75 ℃. Do not exceed 90 ℃
(9) the recommended process for electrolyzing and polishing:
In addition to the oil removal and rust, the electrochemical polishing goes to wash and wash to wash and to wash and to protect.
Electrochemical polishing, water and water
Electrolyte maintenance:
(1) before electrolysis, it must be disused to prevent oil pollution from being contaminated with polish or to cause a large amount of foam in the polishing liquid.
Often measuring the electrolyte density, (2) if the density is small, that water, steam heating to remove excess water, if the density is big, that the moisture is less, can supplement moisture, but need to content determination of other substances, according to the actual situation to add.
(3) the polishing liquid aging: electrolyte in long-term work, the workpiece on the surface of the nickel chrome iron ions dissolved into the polishing liquid solution of iron nickel chromium ion content increased, loss of polishing solution ability, raise the temperature, increase current have no effect, and the best way is to replace the new liquid, can all change, also can be replaced by 80%
(4) regularly clean the cathode and bottom. Stereotype in the process of polishing surface adsorption had thick nickel iron impurities, influence the cathode conductive surface, the current decline, cathodic current density, so to clear out deposits on the cathode board in time. Impurities such as iron nickel chromium affect the li