The repair method grinds off the paint film of the defect area and makes a pinnate side at the end of the contact, filling the hole with the filling and then repainting it.
1 pieces pieces shrink light
The paint film is a semi - light fuzzy state, with a low magnification to observe a large number of fine holes. Sometimes the surface of the paint will be polished.
The reason is that the primer is absorbed by the primer, which is the reason: a) the surface of the porous substrate is precoated or closed, and there is no local spray primer for the atomic dust or the filling of the ashes. B) improper method of painting primer, excessive amount of primer, incorrect, inadequate or poor quality of the material used, and uneven mixing. C) the surface of the primer is not properly handled, and it is polished and treated with no waiting primer. The sandpaper is too thick and the polishing method is not correct. D) its not enough to be completely hardened and sprayed with paint.
Prevent a) properly handle primer surface. B) the thickness of the base coat should be appropriate, and the recommended amount should be used proportionally. Stir well before using. C) after the primer is completely hardened, the surface of the primer shall be smooth and smooth. D) spray paint with enough thickness to be thin and wet for each finish.
After the paint film is completely hardened, it is polished and polished. When the situation is serious, the defect area will be polished and repainted.
2. Dry slow/paint film soft
Describe the drying time of paint film too long or cannot be cured adequately.
The reason why the solvent in the paint is volatile is that: a) the paint film is too thick. B) the environmental conditions of spraying or drying are poor, too cold, too wet, or poor air flow. C) insufficient time in the flow of each paint. D) the amount of the thinner is insufficient, the model is not correct or the quality is poor.
Preve
您可能关注的文档
- 数学笔记(Math notes).doc
- 数学题目(Mathematical subject).doc
- 数据仓库设计过程(Data warehouse design process).doc
- 数学高考基础知识(Basic knowledge of mathematics college entrance examination).doc
- 数据库基本查询语句汇总(Summary of database basic query statements).doc
- 数据库未来展望(Database future outlook).doc
- 数据结构 停车场管理系统(Data structure parking management system).doc
- 数据库第七章(Database 7).doc
- 数据库和ADO笔记(Database and ADO notes).doc
- 数据结构-停车场程序(Data structure-car parking procedures).doc
文档评论(0)