* * * * All the CDC have been annealed under H2 during 2h at 600C as usual. SiC CDC corresponds to particle size from 30 nm, 6 micron and 20 micron chlorinated at 1000C during 3h (except the 30 nm, 10 min) and H2 ann. I did not differentiate them because it was not the purpose. The TiC CDC, KOH activated and the TiC CDC, CO2 act correspond to the data below so you should have all the info. Anthracite is the Spanish material from Linares... Conclusion: We have the same trend at 1 Atm and at 60 Atm, showing that the optimum pore size is 0.6-0.7 nm at any pressure. * * * * * Nanostructured C