2 三:異常孔晶格觀察 異常板晶格結構 正常板晶格結構 從SEM觀察可明顯看出,異常板孔銅結晶出出現大量孿晶晶格結構,且存在晶格空洞異常。 * Copper Clad Laminates business was found in 1985. It is a try for Formosa Group put its toss into the Electronics Materials Div. At that moment, it is just a small unit belong to Nan Ya Plastics Corp., 4th Div. The contribution of sales revenue was just 10% to 4th Plastics Div, and 2% to Nan Ya Plastics Corp. 15 years later, now it is an independent Division of Electronics Material, which has four laminates factories and the other 7 factories produce three basic materials for copper clad laminates. * * * * 2 Nan Ya CC