氧化石墨烯性质及制备.ppt

* Introduction of graphene oxide Graphene Fullerene Carbon Nanotube Graphite H2SO4, KMnO4 A:Peroxide bridge bond B: Hydroxy C:Carboxyl Graphene Oxide (GO) Concentrated H2SO4 Addition of graphene Stirred for 10 min Addition of KMnO4 Stirred for 30 min at 80℃ Addition of H2O Stirred for 6 h at 35℃ Addition of H2O and H2O2 Stirred for 10 min at rt. washed with H2O freeze-dried after sonication Graphene Fullerene Carbon Nanotube Graphite H2SO4, KMnO4 A:Peroxide bridge bond B: Hydroxy C:Carboxyl Graphene Oxide (GO) Introduction of graphene oxide Properties of GO Good water dispersibility