Casting defects
Casting defects in investment steel castings Mould cracking / Finning Surplus metal following contour of crack in shell mould -Excessive drying rate during drying of primary coats -Different coefficients of expansion between primary and subsequent shell coats -Low shell strength -Poor de-waxing Prevention -Reduce shell drying rates -Increase shell green strength ( = polymer additives in binder ) Use compatible refractories Autoclave is best for de-waxing; pressure build-up ought to be less than 10 s If de-waxing by flashfire or with boiling water ? add extra openings to shell Casting
您可能关注的文档
- 拼音五g-k-h.ppt
- 4.5植物的叶与蒸腾作用教案.doc
- 名词性从句20151122公开课定稿.ppt
- 伶官传序课堂用.ppt
- 5、古诗两首精.ppt
- 4.1.3文本信息的结构化.ppt
- 4.5融化与凝固.ppt
- 四年级上第一单元导读.ppt
- 12.2.4待定系数法.pptx
- 做一道拿手菜王燕.ppt
- 基于改进Deeplabv3^(+)的大口黑鲈表型数据测量与品质预测方法.pdf
- 不同色系乌桕呈色期色素含量变化规律.pdf
- 云南干热河谷区柑橘园生草栽培对土壤特性的影响.pdf
- 玉米非生物胁迫适应性的分子机制研究进展:从关键基因到调控网络.pdf
- 生物刺激素对冬瓜幼苗生长的影响.pdf
- 产教融合实训基地助力高质量涉农“双创”型人才培育探索.pdf
- 甜菜碱对热应激山羊胎盘滋养层细胞增殖、凋亡及抗氧化功能的影响.pdf
- 我国荔枝、龙眼新品种保护现状分析及发展对策研究.pdf
- 中国热带农业遥感研究体系框架与展望.pdf
- 基于AMMI模型和GGE双标图评价江苏淮北夏大豆区域试验品种丰产性及适应性.pdf
原创力文档

文档评论(0)