陶瓷检验培训课程[][]

Inspector Training Course 檢驗培訓課程 Light Glaze施釉不夠 Under Fired燒成不夠 Not glossy. A dull or flat finish, undeveloped glaze. 無光澤,晦暗的平的表面,釉面不光滑。 (Not to be confused with satin or matte finishes used for decorative purposes.)不要和高級的,裝飾用的表面混淆。 Metal Spots金屬點 An area of contrasting color less than 1/32 in. (0.031 in.) in maximum dimension. Spots/specks are often black or green in color.顏色不一致,最大1/32英吋,斑點一般是黑色或綠色。 Finish拋光缺陷 Marks in the fired piece that are not part of the original design lines. Includes pallet marks, dents, etc.成品上的標記,不是原來設計的,包括Pallet,標記,凹痕。 Scratch (Before Firing)燒成前劃痕 A scr