钙钛矿太阳能电池制作过程(图)复习课程.pptVIP

  • 108
  • 0
  • 约1.21千字
  • 约 16页
  • 2018-04-27 发布于天津
  • 举报

钙钛矿太阳能电池制作过程(图)复习课程.ppt

钙钛矿太阳能电池制作过程(图)复习课程.ppt

Logo Logo OTPs Solar Cells Wang W.P. 2016-10-21 1. 视频实验整理(湿度影响,材料PbCl2+CH3NH3I) 相对湿度:30 % 相对湿度:60 % Processing in an environment with a humidity of 30-40% rh results in films having a bright yellow colour post spin coating. Placing these films on a 90°C hotplate initially maintains this film colour and after 90-120 minutes, a perovskite film will be formed with a dark brown/grey colour If, instead, the humidity of the environment is too high (40% rh) then the film colour will appear orange/brown after the 30 second spin coating stage. Although the film will revert back to a bright yellow upo

文档评论(0)

1亿VIP精品文档

相关文档