* * This is a typical concrete mix design . It contains 450 kg of cement which is unfortunately for Lafarge very rarely the case in practical ! . Here one can explain that the water to cement factor is 0,4 which represents the exact amount of water required for the hydration of the cement . Once the hydration is completed the concrete will have a very litle porosity and will be very durable . The problem which occurs most of the time is that people reduce the amount of cement ( less expensive concrete ) and because it is not possible to reduce the water the W/C ratio increases.In the end , th