《Infrared brazing of Ti50Ni50 shape memory alloy using two Ag–Cu–Ti active braze alloys》.pdf

《Infrared brazing of Ti50Ni50 shape memory alloy using two Ag–Cu–Ti active braze alloys》.pdf

  1. 1、本文档共9页,可阅读全部内容。
  2. 2、原创力文档(book118)网站文档一经付费(服务费),不意味着购买了该文档的版权,仅供个人/单位学习、研究之用,不得用于商业用途,未经授权,严禁复制、发行、汇编、翻译或者网络传播等,侵权必究。
  3. 3、本站所有内容均由合作方或网友上传,本站不对文档的完整性、权威性及其观点立场正确性做任何保证或承诺!文档内容仅供研究参考,付费前请自行鉴别。如您付费,意味着您自己接受本站规则且自行承担风险,本站不退款、不进行额外附加服务;查看《如何避免下载的几个坑》。如果您已付费下载过本站文档,您可以点击 这里二次下载
  4. 4、如文档侵犯商业秘密、侵犯著作权、侵犯人身权等,请点击“版权申诉”(推荐),也可以打举报电话:400-050-0827(电话支持时间:9:00-18:30)。
查看更多
《Infrared brazing of Ti50Ni50 shape memory alloy using two Ag–Cu–Ti active braze alloys》.pdf

Intermetallics 14 (2006) 630–638 /locate/intermet Infrared brazing of Ti50Ni50 shape memory alloy using two Ag–Cu–Ti active braze alloys R.H. Shiue, S.K. Wu * Department of Materials Science and Engineering, National Taiwan University, Taipei 106, Taiwan, ROC Received 30 June 2005; accepted 24 October 2005 Available online 4 January 2006 Abstract Microstructural evolution, shape memory effect and shear strength of infrared brazed Ti50Ni50 shape memory alloy using Cusil-ABAw and Ticusilw active braze alloys are investigated. The Ag–Cu eutectic braze alloy can readily wet Ti50Ni50 substrate by minor titanium additions. The brazed Ti50Ni50/Cusil-ABAw/Ti50Ni50 joint is mainly comprised of Cu-rich, Ag-rich and CuNiTi phases. On the other hand, the brazed Ti50Ni50/Ticusilw/Ti50Ni50 joint consists of Ag-rich, Cu-rich and TiCu 2 phases. Because the chemical composition of Ticusil braze alloy is located inside the huge miscibility gap, the molten braze tends to be separated into two liquids during brazing. One is rich in Ag, and the other is rich in both Cu and Ti. The Ag-rich liquid does not react with Ti50Ni50 substrate. In contrast, the copper content is depleted from the matrix of brazed joint due to the formation of interfacial TiCu 2 phase. The TiCu2 phase is less detrimental to the shape memory effect than CuNiTi phase during the shape recovery bending test. Shear strength of brazed joints exceeds 200 MPa for both braze alloys if the brazing time exceeds 180 s. However, thick interfacial CuNiTi and TiCu2 layers can deteriorate the