STUDY ON THE NEW TECHNOLOGY OF THE FLOATATION
SEPARATION OF ZINC AND COPER SULFIDE MINERALS OF Liwu
ABSTRACT
There is an increasing demand for zinc and coper metals as a major raw material with the
development of economy and it becomes urgently necessary to exploit refractory zinc and coper
ores as the easily-separate zinc and coper ores increasingly reduce.
Zinc and coper sulfide metals of Liwu were studied in this subject, the mineralogy of sample
indicates that the test material belongs to refractory metallic sulphide ore, with the primary
minerals in the materials being chalcopyrite, marmatite and pyrrhotite. The efficient
concentration of copper is achieved using the new copper collector LP-01 in a mild slurry
medium, without the negative effect for marmatite depression due to high alkali medium during
copper flotation; and the zinc-sulphide is also successfully achieved by controlling the pH values
of slurry mediums at around 9.5 during roughing stage and at 10~11 during reconcentrating stage,
respectively. This technology has obtained relatively qualified copper concentrate and zinc
concentrate while applied in industry. The ore contain 1.42% Cu 、0.98% Zn, then the copper
concentrate which contain 25.91% Cu、1.08% Zn is received, and the recovery of Cu is 9 1.42%;
the zinc concentrate which contain 2.09% Cu 、33.22% Zn is received, and the recovery of Zn is
45.76%.
Industrial tests of this technology put up in concentration plant of LiWu copper ore
company in Sichuan at May 2007, the result of industrial tests show that the copper concentrate
which contain 24.85% Cu、1.15% Zn is received, as the green ore contain 1.38% Cu 、1.01% Zn,
the recovery of Cu is