PPA的应用 Recommendations in PE film extrusion Step 1: Create the PPA coating by running the line for 20-30 minutes with 5% of masterbatch (containing 2 to 5% of PPA).Step 2: Then reduce the concentration to 1wt% of masterbatch. PPA的应用 Recommendations in HDPE blow molding Step 1: Create the PPA coating by running the line for 20-30 minutes with 5% of masterbatch (containing 2 to 5% of PPA).Step 2: Then reduce the concentration to 1wt% of masterbatch and wait for the line to stabilize.Step 3: Reduce extrusion temperature by and wait for the line to stabilize.Step 4: Reduce cycle time by