注塑模具则中英文对照版
Document Owner: Lawrence Chung
Maintained by: HK PDM
REVISION DESCRIPTION OF CHANGE CHANGE NO. DATE RELEASED 1 Initial Release 26222 May 2006 (See Agile)
APPROVALS OBTAINED IN AGILE
Injection Molding Guideline
1. Plastic Material
Assume the general purpose grade plastic materials to be used for our molding
In case of special grade materials, please list the material grade brand on our tool plan
All the plastic materials for molding must be same as the materials during development stage.
In case of material shortage or cost issue, the new sourced material shall be tested and confirmed acceptable prior use.
2. Colorant
All the colorant must be conformed to heavy elements directives for both ASTM F963 EN71.
Most of the dry pigments are hygroscopic; they must be properly sealed after use.
For the components with high color consistence, the masterbatches or pre-color plastic materials are required.
3. Regrind Material Ratio
For plastic material on structural components, no regrind is allowed
For general purpose material on non structural components, 20% maximum runner regrind can be blended with virgin material.
For those translucent or true white color components, no regrind is allowed.
For short glass filled materials, 15% maximum regrind can be blended with virgin material
For long glass filled materials, no regrind is allowed.
The maximum number of regrind passes for general purpose materials shall be 3.
Only 1 time of regrind pass is allowed for short glass reinforced materials
The regrind ratio shall be shown in our updated tool plan to follow.
The regrind ratio and no. of regrind passes has to be validated and confirmed during development stage. If not, no regrind will be allowed.
?Burned or discolored sprues or parts must not be used as regrind.
Hot nozzle hot runner is our preference to eliminate runner scrap.
4. Material Drying
Most plastic resins require thorough drying prior injection molding to assure maximum properties in the molded pa
您可能关注的文档
- 汽车知识松入门.doc
- 汽车知识赛题库.doc
- 汽车电气训中心仪器.doc
- 汽车知识门大全,看了之后我才真正了解汽车.doc
- 汽车维修S推行手册.doc
- 汽车维修业实施性教学计划.doc
- 汽车维修全生产、应急预案等大全.doc
- 汽车维修展出路在何方.doc
- 汽车维修格结算员类题库.doc
- 汽车维修美容.doc
- GB/T 32151.38-2024温室气体排放核算与报告要求 第38 部分:水泥制品生产企业.pdf
- 中国国家标准 GB/T 32151.38-2024温室气体排放核算与报告要求 第38 部分:水泥制品生产企业.pdf
- 《GB/T 22069-2024燃气发动机驱动空调(热泵)机组》.pdf
- GB/T 22069-2024燃气发动机驱动空调(热泵)机组.pdf
- 中国国家标准 GB/T 22069-2024燃气发动机驱动空调(热泵)机组.pdf
- 中国国家标准 GB/T 11064.1-2024碳酸锂、单水氢氧化锂、氯化锂化学分析方法 第1部分: 碳酸锂含量的测定 滴定法.pdf
- GB/T 11064.1-2024碳酸锂、单水氢氧化锂、氯化锂化学分析方法 第1部分: 碳酸锂含量的测定 滴定法.pdf
- 《GB/T 11064.1-2024碳酸锂、单水氢氧化锂、氯化锂化学分析方法 第1部分: 碳酸锂含量的测定 滴定法》.pdf
- GB/T 1148-2024内燃机 铝活塞.pdf
- 中国国家标准 GB/T 1148-2024内燃机 铝活塞.pdf
文档评论(0)