硒酸泥制备粗硒新工艺
李倩;张宝伸文前;杨兴文
【摘要】 Crude selenium was prepared from selenium acid mud using a new technology of kerosene desulphurization, oxidization-leaching and reduction-extraction of selenium. The results show that kerosene can effectively remove sulfur from selenium acid mud when the temperature is controlled above 95°C, and the rate of desulphurization is larger than 97%. Accordingly, the optimum oxidization-leaching conditions are determined as follows: temperature 80C, leaching time 2 h and ratio of liquid to solid of 5:1, H2SO4 concentration 300 g/L. After oxidization-leaching under optimu
您可能关注的文档
最近下载
- 宣贯培训(2026年)《GBT 24892-2010动植物油脂 在开口毛细管中熔点(滑点)的测定》.pptx VIP
- 雪茄持灰大赛活动策划方案.pptx
- 路面设计原理-国外设计方法-01-AASHTO路面结构设计指南_101-200.docx VIP
- 路面设计原理-国外设计方法-01-AASHTO路面结构设计指南_1-100.docx VIP
- 一种可拆卸式外窗防风装置.pdf VIP
- 国家标准 GBT 24892-2010 动植物油脂在开口毛细管中熔点(滑点)的测定.pdf
- 三一全地面起重机SAC5000T7_产品手册用户使用说明书技术参数图解图示电子版.pdf VIP
- 2025至2030中国造口护理和和造口护理及配件行业产业运行态势及投资规划深度研究报告.docx
- 实施指南《GB18436 - 2022轮机日志和车钟记录簿》实施指南.pptx VIP
- 四川大学《微积分II-2》2023-2024学年第二学期期末试卷.pdf VIP
原创力文档

文档评论(0)